DuPont Hytrel® HTR8303 Thermoplastic Copolyester Elastomer (TPC-ET)
Subcategory: Polyester, TP; Elastomer, TPE; Thermoplastic
Material Notes: Hytrel® HTR8303 is a thermoplastic polyester elastomer with excellent high temperature properties and hydrolytic stability designed for extrusion coating applications. This polymer has a durometer hardness of 65D and a flexural modulus of 750MPa.
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Dielectric Constant
- Dissipation Factor
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Oxygen Index
- Melt Temperature
- Appearance
- DuPont Product Category
- Form
- Processing Method
- Region
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|