DuPont Rynite® PCR108 BK515 PET
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Rynite® PCR108 BK515 is a 30% glass fiber reinforced resin based on 100% post consumer recyclate PET and modified for improved impact resistance.
| Available Properties |
- Density
- Filler Content
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Dielectric Strength
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Appearance
- DuPont Product Category
- Form
- Processing Method
- Region
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|