DuPont Rynite® RE15022 NC010 PET
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic
Material Notes: Rynite® RE15022 NC010 is a 36% glass reinforced product designed for applications that need high burst strength.
| Available Properties |
- Specific Gravity
- Filler Content
- Tensile Strength, Ultimate
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Unnotched
- Charpy Impact Unnotched
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Appearance
- Form
- Region
|
|
|
|
| Property Data |