DuPont Thermx® CG943 NC010T PCT
Subcategory: Polyester, TP; Thermoplastic; Polycyclohexylenedimethylene Terephthalate (PCT)
Material Notes: Thermx® CG943 NC010T is a 40% glass fiber reinforced, flame retardant polycyclohexylenedimethylene terephthalate resin for injection molding.