DuPont Vespel® CP0301 Polyimide
Subcategory: Polyimide; Thermoplastic
Material Notes: Sheet molding compounds consisting of long chopped fibers held in a variety of polymer matrices. Superior strength, light weight applications for aircraft clamps and structural components.
| Available Properties |
- Specific Gravity
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Glass Temperature
- Heat Stabilized
- Region
|
|
|
|
| Property Data |