DuPont Vespel® CP0801 Polyimide
Subcategory: Polyimide; Thermoplastic
Material Notes: Braided series of graphite, carbon, glass, and Teflon® fibers, in hollow braids combined with polyimides to produce bushings that offer toughness, thermal and wear resistance.
| Available Properties |
- Specific Gravity
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Strength
- Glass Temperature
- Heat Stabilized
- Region
|
|
|
|