DuPont Zenite® 7140X NC010 LCP
Subcategory: Liquid Crystal Polymer (LCP); Thermoplastic
Material Notes: Zenite® 7140X NC010 is a 40% glass reinforced liquid crystal polymer resin with improved weldline strength, low post soldering warpage and a heat deflection temperature of 298ºC.
| Available Properties |
- Density
- Filler Content
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Appearance
- DuPont Product Category
- Form
- Part Marking Code
- Region
- Resin Identification
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|