DuPont Zenite® ZE55801 NC010 LCP
Subcategory: Liquid Crystal Polymer (LCP); Thermoplastic
Material Notes: Zenite® ZE55801 NC010 is a 30% glass reinforced, lubricated liquid crystal polymer resin designed for enhanced electroless plating.
| Available Properties |
- Specific Gravity
- Filler Content
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- CTE, linear 100°C
- CTE, linear 250°C
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Appearance
- DuPont Product Category
- Form
- Part Marking Code
- Region
- Resin Identification
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|