DuPont Zytel® 450HSLX BK152 Nylon 66
Subcategory: Nylon; Thermoplastic; Nylon 66
Material Notes: Zytel® 450HSLX is a heat stabilized, lubricated, medium toughened polyamide 66 for injection molding. It has high impact resistance at low temperature and dry as molded.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Drying
- DuPont Product Category
- Form
- Region
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|