DuPont Zytel® BM73G15THS BK317 Nylon 6
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Zytel® BM73G15THS is a 15% glass fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for blow molding.
| Available Properties |
- Density
- Filler Content
- Linear Mold Shrinkage
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Appearance
- Drying
- DuPont Product Category
- Form
- Region
|
|
|
|