DuPont Zytel® FN714 NC010 Nylon 66
Subcategory: Nylon; Thermoplastic; Nylon 66
Material Notes: Zytel® FN714 NC010 is an impact modified, very flexible, plasticizer free polyamide 66 resin having good heat aging and chemical resistance.
| Available Properties |
- Density
- Specific Gravity
- Water Absorption
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Tensile Impact Strength
- Izod Impact, Notched
- Volume Resistivity
- Melting Point
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Additive
- Appearance
- Drying
- DuPont Product Category
- Features
- Form
- Injection Moldable
- Part Marking Code
- Processing Method
- Region
- Resin Identification
- Uses
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|