DuPont Zytel® FN727 NC010 Nylon 6
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Zytel® FN727 NC010 is an impact modified, plasticizer free, very flexible polyamide 6 alloy resin having good low temperature toughness, good heat aging and good chemical resistance. Uses include cable jacketing, hose and tube applications.
| Available Properties |
- Density
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact, Notched
- Tensile Impact Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Appearance
- Drying
- DuPont Product Category
- Form
- Part Marking Code
- Processing Method
- Region
- Resin Identification
- Uses
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|