DuPont Zytel® HTN51G45HSLR BK420 Polyphthalamide (PPA)
Subcategory: Polyphthalamide; Thermoplastic
Material Notes: Zytel® HTN51G45HSLR BK420 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin with improved hydrolysis resistance. It is also a PPA resin.
| Available Properties |
- Density
- Filler Content
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Additive
- Appearance
- DuPont Product Category
- Features
- Form
- Processing Method
- Region
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|