DuPont Zytel® HTN53G50HSLRHF BK083 Polyamide, High Performance (HPPA)
Subcategory: Nylon; Thermoplastic
Material Notes: Zytel® HTN53G50HSLRHF BK083 is a 50% glass reinforced, lubricated high performance polyamide resin with improved flow, developed for structural applications requiring excellent surface appearance with water-heated molds.
| Available Properties |
- Density
- Filler Content
- Water Absorption
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Additive
- Appearance
- DuPont Product Category
- Form
- Part Marking Code
- Processing Method
- Region
- Resin Identification
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|