DuPont Zytel® HTN53GM40HSL BK083 Polyamide, High Performance (HPPA)
Subcategory: Nylon; Thermoplastic
Material Notes: Zytel® HTN53GM40HSL BK083 is a 40% glass and mineral reinforced, heat stabilized, lubricated high performance polyamide resin, developed for moderate temperature, low warp structural applications.
| Available Properties |
- Density
- Filler Content
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Additive
- Appearance
- Drying
- DuPont Product Category
- Form
- Heat Stabilized
- Injection Moldable
- Part Marking Code
- Processing Method
- Region
- Resin Identification
- Ultrasonic Weldable
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|