DuPont Zytel® HTN54G50HSLR BK031 Polyphthalamide (PPA)
Subcategory: Polyphthalamide; Thermoplastic
Material Notes: Zytel® HTN54G50HSLR BK031 is a 50% glass reinforced, toughened, heat stabilized, hydrolysis resistant high performance polyamide resin developed for retention of toughness and stiffness with moisture in structural applications. It is also a PPA resin.
| Available Properties |
- Density
- Filler Content
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Additive
- Appearance
- DuPont Product Category
- Features
- Form
- Part Marking Code
- Processing Method
- Region
- Resin Identification
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|