DuPont Surlyn® 9120 Ionomer Resin, Zinc
Subcategory: Ionomer; Thermoplastic
Key Words: Ethylene/Methacrylic Acid (E/MAA) Copolymer
Material Notes: Surlyn® 9120 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutralization levels for this grade are optimized to deliver exceptional low-temperature toughness. The resin is highly suitable as a polymer modifier, to increase toughness. Surlyn® 9120 can be injection or blow molded, and is processable by extrusion into sheets or shapes.Data provided by the manufacturer.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Abrasion
- Melting Point
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|