DuPont Surlyn® 9520 Ionomer Resin, Zinc
Subcategory: Ionomer; Thermoplastic
Key Words: Ethylene/Methacrylic Acid (E/MAA) Copolymer
Material Notes: Surlyn® 9520 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutralization levels for this grade are optimized to deliver low temperature toughness. The resin can be injection or blow molded, and is processable by extrusion into sheets or shapes. However, its main application is as a engineering resin modifier: It improves the toughness of nylon 6 and 6/6 resins. The resin complies with the provisions of U.S. Food and Drug Administration (FDA) Title 21 Code of Regulations 177:1330 - ionomer resins.Data provided by the manufacturer.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Tensile Impact Strength
- Abrasion
- CTE, linear 20°C
- Thermal Conductivity
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
- Flammability Test
- Haze
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|