DuPont Surlyn® 1652SBR Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
Subcategory: Ionomer; Thermoplastic; Polymer
Key Words: Ethylene/Methacrylic Acid (E/MAA) Copolymer
Material Notes: Surlyn® 1652SBR is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to process polyethylene resins. Applications: Meat, poultry, seafood and cheese packaging; Cereal liners; Medical/pharmaceutical packaging; Powdered/granular food and nonfood pouches; Edible oil, motor oil, and other liquid product pouches; Snack structuresData provided by the manufacturer, DuPont Packaging.
| Available Properties |
- Density
- Melt Flow
- Seal Strength
- Hot Tack Strength
- Melting Point
- Vicat Softening Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|