DuPont Teijin Films Mylar® LB Polyester Film, 75 Gauge (19 µm)
Subcategory: Polyester, TP; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. An uncoated, transparent polyester film designed for use as a component of a lamination. Standard thickness offered include 48, 75, and 92 gauges. Varieties with enhanced surface characteristics for bonding by inks, primers, and adhesives. A basic lamination would combine plain or printed LB with a heat sealable ply consisting of LDPE, LLDPE, EVA, ionomer, acid copolymer, PVC, or other materials using adhesive or extrusion laminating techniques.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Modulus of Elasticity
- Tear Strength Test
- Maximum Service Temperature, Air
- Haze
- Gloss
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|