DuPont Teijin Films Mylar® M30 Polyester Film, 100 Gauge (25 µm), PVDC Coated
Subcategory: Polyester, TP; PVDC; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and oxygen barrier. Available in 50, 75, and 100 gauges. Used both in unsupported form, or as a component of a lamination, and can be run on both form-fill-seal and overwrap equipment. It is particularly well suited for the packaging of long shelf life or moisture-and oxygen-sensitive products.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Linear Mold Shrinkage
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Modulus of Elasticity
- Tear Strength Test
- Seal Strength
- Maximum Service Temperature, Air
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|