DuPont Teijin Films Mylar® 50 M44E Polyester Film, One-Sided PVDC Barrier Coated, 50 Gauge
Subcategory: Polyester, TP; PVDC; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. A transparent, exceptionally strong polyester film, coated on one side with an oxygen and moisture barrier PVDC copolymer. It is used as a substrate in combination with sealant webs, to produce a highly durable structure with excellent oxygen barrier. Can be printed with appropriate inks, including water based. The barrier coating may be adversely affected by certain solvents, if they are trapped during printing or laminating.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Linear Mold Shrinkage
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Modulus of Elasticity
- Tear Strength Test
- Maximum Service Temperature, Air
- Haze
- Gloss
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|