DuPont Teijin Films Mylar® LBT Polyester Film, 48 Gauge (12 µm)
Subcategory: Polyester, TP; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. An uncoated, transparent polyester film that has been corona-treated to provide superior wetting and adhesion to inks, primers, and adhesives. Standard thicknesses include 48, 75, and 92 gauges. Other gauges may be available on special request. Typically used as the reverse printed outer ply of a lamination with inner plies providing additional oxygen barrier if needed, as well as heat sealability.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Linear Mold Shrinkage
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Modulus of Elasticity
- Tear Strength Test
- Maximum Service Temperature, Air
- Haze
- Gloss
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|