DuPont Teijin Films Mylar® M45 Polyester Film, 75 Gauge (22 µm), PVDC Coated
Subcategory: Polyester, TP; PVDC; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. A transparent polyester packaging film, dispersion coated on one side with a PVDC copolymer. The coating is an excellent moisture and oxygen barrier. M45 is designed to be combined with a sealant layer, locking in the PVDC coating. M45 can be surface or reverse printed with appropriately formulated inks, and can be combined with other webs by adhesive or extrusion laminating. The coated surface is particularly well suited for water based inks and adhesives.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Linear Mold Shrinkage
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Modulus of Elasticity
- Tear Strength Test
- Maximum Service Temperature, Air
- Haze
- Gloss
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|