DuPont Sclairfilm® GL-1 LLDPE Film, Laminating, 50.8 µm Thickness
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Key Words: Linear Low Density Polyethylene; DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal and hot tack characteristics along with good physical strength and opticals.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Film Tensile Strength at Break, MD
- Film Elongation at Break, MD
- Tensile Modulus
- Dart Drop Test
- Haze
- Gloss
|
|
|
|
| Property Data |