DuPont Sclairfilm® LWS-1 LMDPE Film, Laminating, 50.8 µm Thickness
Subcategory: Polyethylene; Thermoplastic; MDPE; Polymer
Key Words: Linear Medium Density Polyethylene; DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one side for both ink and adhesive bonding properties. For laminating to other substrates such as Dartek nylon film or Mylar polyester film for heat-in-bag or boil-in-bag applications.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Film Tensile Strength at Break, MD
- Film Elongation at Break, MD
- Tensile Modulus
- Dart Drop Test
- Seal Strength
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|