DuPont Dartek® F-101 Nylon 6,6 Forming Film, 25 µm Thickness
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Key Words: Nylon 66, Polyamide 66; DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. A cast nylon film made from type 6,6 polymer - the condensation product of adipic acid and hexamethylen diamine. It contains all the excellent properties historically found in Dartek®. Can be printed, laminated or extrusion coated. In converter combinations it may be used in any packaging end use which requires thermoforming, be it by vacuum, compressed air or mechanical means.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop Test
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|