DuPont Dartek® O-401 Nylon 6,6 Oriented Film, 15 µm Thickness
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Key Words: Nylon 66, Polyamide 66; DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. A machine direction oriented nylon type 6,6 film. Many of the properties of nylon 6,6 film are improved upon orientation, but particularly the overall toughness and gas permeability. Provides excellent qualities to the converter which make it an ideal film for printing and laminating. Its barrier properties and stiffness make it an excellent choice for a variety of packaging end uses such as snacks, processed meat, cheese, condiments.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|