DuPont Dartek® B-602 Nylon 6,6 Barrier Film, 38 µm Thickness, PVDC Coated
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Key Words: Nylon 66, Polyamide 66; DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. A strong, transparent nylon 6,6 film which has a PVDC coating applied to one side for enhanced barrier to oxygen, moisture, grease and odor. It is specially formulated for use in high humidity applications. Can be printed, laminated, or extrusion coated. In converter combinations, it can be used for any packaging or industrial end use requiring high barrier properties. It can be easily thermoformed for assorted shapes and products such as meats and cheeses.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop Test
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|