DuPont Dartek® N-201 Nylon 6,6 Non-Forming Film, 25 µm Thickness
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Key Words: Nylon 66, Polyamide 66; DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. A nylon film made from type 6,6 polymer - the condensation product of adipic acid and hexamethylene diamine. Primarily formulated for pouch and primal bag applications and is not recommended, nor guaranteed for thermoforming. However, it does provide barrier to oils, greases and odors, has low permeability to oxygen and good overall physical properties.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop Test
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|