DuPont Clysar® EHC Polyolefin Shrink Packaging Film, 150 Gauge
Subcategory: Polyethylene; Polypropylene; Thermoplastic; Polymer
Key Words: Polyethylene, Polypropylene; DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when excellent optics, high shrink force, and superb sheet flatness are essential. An excellent choice for doing multi-packs, high-speed applications, and static sealing.
| Available Properties |
- Oxygen Transmission
- Film Tensile Strength at Break, MD
- Film Elongation at Break, MD
- Modulus of Elasticity
- Coefficient of Friction
- Elmendorf Tear Strength MD
- Seal Strength
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|