DuPont Teijin Films Melinex® 813 Polyester Packaging Film, 48 Gauge
Subcategory: Polyester, TP; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. Melinex® 813 is a polyester film, pretreated on one side to provide excellent adhesion to a wide range of both solvent- and water-based inks. Melinex® 813 film provides good clarity for reverse printing and allows inks to shine through with high quality. The film's pretreated surface also provides improved adhesion for various coatings and adhesives, often eliminating the need for any type of priming operation. The chemical pretreatment on Melinex® 813 film does not result in a performance or shelf life decline over time, and generally is superior to corona treated film. Melinex® 813 film features good clarity and handling characteristics in metallizing operations. When aluminum metallized, the film exhibits excellent aesthetic quality as well as the best barrier to oxygen and moisture in a flexible packaging film. Melinex® 813 is a polyester base film that is compliant with the U.S. Food and Drug Administration regulations under 21 CFR 177.1630, Sections (f) and (g), which is treated on one side with a coating which also is in compliance with 21 CFR 177.1630. Melinex® 813 may be used for packaging, transporting or holding food (excluding alcoholic beverages) at temperatures not to exceed 250°F; and for packaging, transporting or holding alcoholic beverages that do not exceed 50 percent alcohol by volume.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Coefficient of Friction
- Coefficient of Friction, Static
- Haze
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|