DuPont Teijin Films Mylar® RL43 Polyester Packaging Film, 50 Gauge
Subcategory: Polyester, TP; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. Mylar® RL43 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. Mylar® RL43 is designed to produce strong heat seals to polypropylene (PP). Although designed especially to seal to polypropylene, Mylar® RL43 will produce strong seals to a broad range of container substrates including amorphous polyester (APET, also PETG), semicrystalline polyester (CPET), polyester coated paperboard, polyvinylchloride (PVC), polyethylene (HDPE), and polystyrene (HIPS). Mylar® RL43 has the same type heat seal layer as Mylar® RL42, but the seal layer is thicker than Mylar® RL42. Mylar® RL43 produces the highest seal strengths to polypropylene of Mylar® lidding films and tends to produce tearing seals to non-polar substrates under chilled conditions. Mylar® RL43 is recommended when light caulking is needed. Mylar® RL43, like other RL types, has a lower seal initiation temperature than lidding films with an amorphous polyester heat seal layer (e.g., Mylar® OL, OL2). This allows good seals to be made at higher line speeds (or using lower sealing temperatures).
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus
- Tear Strength Test
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|