DuPont Teijin Films Mylar® OB12AF Polyester Packaging Film, 50 Gauge
Subcategory: Polyester, TP; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. Mylar® OB12AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the opposite side of the film from the heat seal layer. Mylar® OB12AF is essentially Mylar® OL12 with a barrier layer. Mylar® OB12AF is dual ovenable film which provides strong, aggressive seals to polar substrates such as amorphous polyester (APET, also PETG), semicrystalline polyester (CPET), polyester coated paperboard, and polyvinylchloride (PVC). Mylar® OB12AF does not seal to polyethylene, polypropylene, or polystyrene. DuPont Teijin Films offers another family of lidding films (RB types) for sealing to these substrates. Mylar® OB12AF has higher hot tack and a thicker seal layer than either Mylar® OB02 or OL2, and can be used in hot fill applications. It is not recommended for applications requiring retort sterilization. Mylar® OB12AF lidding films have excellent grease and oil resistance. Heat seals produced with Mylar® OB12AF are stronger than with Mylar® OL2 and may be difficult to peel without shredding at any gauge. Mylar® OB12AF is recommended for applications needing a lidding film which heat seals like Mylar® OL12AF, but with much lower permeability to gases (oxygen, carbon dioxide) and moisture. Mylar® OB12AF lidding films are available with anti-fogging capability to provide better clarity when stored and displayed in refrigerated conditions.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus
- Tear Strength Test
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|