DuPont Teijin Films Mylar® RB5 Polyester Packaging Film, 50 Gauge
Subcategory: Polyester, TP; Thermoplastic; Polymer
Key Words: DuPont Packaging Polymers
Material Notes: Data provided by DuPont Packaging Polymers. Mylar® RB5 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer and a polyvinylidene chloride (PVDC) barrier layer "buried" between the OPET base and the EVA heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Mylar® RB5 is designed to seal to a broad range of container substrates including amorphous polyester (APET, also PETG), semicrystalline polyester (CPET), polyester coated paperboard, polyvinylchloride (PVC), polyethylene (HDPE), polypropylene (PP), and polystyrene (HIPS). Mylar® RB5 has the same type and thickness of heat seal layer as Mylar® RL32. The heat seal strengths of Mylar® RB5 are intermediate between Mylar® RL31 and Mylar® RL33. Like Mylar® RL32, Mylar® RB5 has a lower seal initiation temperature than lidding films with an amorphous polyester heat seal layer (e.g., Mylar® OL, OL2). This allows good seals to be made at higher line speeds (or using lower sealing temperatures).
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus
- Tear Strength Test
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|