DuPont Elvamide® 8066 Low Melt Point Nylon Multipolymer Resin

 

Subcategory: Nylon; Thermoplastic; Nylon, Other

Key Words: Polyamide

Material Notes:
Used in textile adhesive market.

The Elvamide® nylon multipolymer resins are thermoplastic polyamides that combine the inherent toughness of nylon with ease of processing in solvent as well as melt systems. Elvamide® resins differ from conventional nylons in that they offer alcohol solubility, lower melt-processing temperatures, excellent elongation, and ability to cross-link with thermosetting resins,

Elvamide® resins can be used singly or in a combination and can be further modified by formulating with plasticizer or other resins to meet specific end-use requirements. For most uses, they are applied from solvent solutions. They can also be melt compounded as, for example, in the manufacture of pigment concentrates or for extrusion into film adhesives for heat reactivation. Their relatively low melt-processing temperature allows use with heat-sensitive pigments and substrates.

Like Zytel® nylon resins, Elvamide® nylon multipolymer resins are suitable for molding and extrusion. They are tough, withstand impact and resist abrasion, but are softer and more flexible than conventional nylons. Melting points for Elvamide® multipolymer resins range from 115°C to 160°C, compared with 265°C for high temperature resistant nylon homopolymer.

Available Properties
  • Density
  • Water Absorption
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。