DuPont Teflon® PTFE Grade 7A Granular Molding Powder

 

Subcategory: Fluoropolymer; Thermoplastic; PTFE

Close Analogs: Data provided by the manufacturer.

Key Words: Polytetrafluoroethylene; DuPont Fluoroproducts

Material Notes:
Teflon® PTFE white granular molding powders are ideal for molding many different end products and stock shapes. Excellent chemical resistance, electrical properties, high temperature performance, low temperature toughness, plus unique adhesion and flame resistance.

Teflon® PTFE granular molding powders are processed by compressing them into a desired shape and heating them at temperatures above their melting point to consolidate the powder.

Resin Characteristics: High bulk density. These small particles result in the highest quality electrical and mechanical properties of all Teflon® PTFE granular molding powders. Uses: Large cylinders for making tape or sheet by skiving; large shapes for machining or direct use.

Typical properties for Teflon® PTFE Granular Resin:

Available Properties
  • Specific Gravity
  • Bulk Density
  • Water Absorption
  • Particle Size
  • Linear Mold Shrinkage
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Flexural Modulus
  • Coefficient of Friction
  • Izod Impact, Notched
  • Volume Resistivity
  • Surface Resistivity per Square
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Arc Resistance
  • Melting Point
  • Flammability, UL94
  • Oxygen Index
  • Drying Temperature
  • 20% Hydrochloric Acid Transmission, g/100sq in.
  • 50% Sodium Hydroxide Transmission, g/100sq in.
  • Acetic Acid Transmission, g/100sq in.
  • Acetone Transmission, g/100sq in.
  • Acetophenone Transmission, g/100sq in.
  • Benzene Transmission, g/100sq in.
  • Carbon Tetrachloride Transmission, g/100sq in.
  • Chemical/Solvent Resistance
  • Detergent Resist. on grit-blasted aluminum, Hours
  • Detergent Resistance on aluminum, Hours
  • Detergent Resistance on grit-blasted steel, Hours
  • Etyl Acetate Transmission, g/100sq in.
  • Folding Endurance, # cycles, .18-.20 mm
  • Heat of Combustion J/g
  • Hexane Transmission, g/100sq in.
  • Piperidine Transmission, g/100sq in.
  • Red Fuming Nirtric Acid Transmission, g/100sq in.
  • Salt Spray Resistance on aluminum, Hours
  • Salt Spray Resistance on steel, Hours
  • Sulfuric Acid Transmission, g/100sq in.
  • Water Transmission, g/100sq in.
  • Weather Resistance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。