DuPont Teflon® PTFE Grade 7C Granular Molding Powder
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Close Analogs: Data provided by the manufacturer.
Key Words: Polytetrafluoroethylene; DuPont Fluoroproducts
Material Notes: Teflon® PTFE white granular molding powders are ideal for molding many different end products and stock shapes. Excellent chemical resistance, electrical properties, high temperature performance, low temperature toughness, plus unique adhesion and flame resistance. Teflon® PTFE granular molding powders are processed by compressing them into a desired shape and heating them at temperatures above their melting point to consolidate the powder. Resin Characteristics: Small, fibrous particles with a low bulk density Uses: Usually mixed with inorganic powders to make filled molding compounds that offer improved wear and cold flow resistance. Typical properties for Teflon® PTFE Granular Resin:
| Available Properties |
- Specific Gravity
- Bulk Density
- Water Absorption
- Particle Size
- Linear Mold Shrinkage
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Coefficient of Friction
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistivity per Square
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Melting Point
- Flammability, UL94
- Oxygen Index
- Drying Temperature
- 20% Hydrochloric Acid Transmission, g/100sq in.
- 50% Sodium Hydroxide Transmission, g/100sq in.
- Acetic Acid Transmission, g/100sq in.
- Acetone Transmission, g/100sq in.
- Acetophenone Transmission, g/100sq in.
- Benzene Transmission, g/100sq in.
- Carbon Tetrachloride Transmission, g/100sq in.
- Chemical/Solvent Resistance
- Detergent Resist. on grit-blasted aluminum, Hours
- Detergent Resistance on aluminum, Hours
- Detergent Resistance on grit-blasted steel, Hours
- Etyl Acetate Transmission, g/100sq in.
- Folding Endurance, # cycles, .18-.20 mm
- Heat of Combustion J/g
- Hexane Transmission, g/100sq in.
- Piperidine Transmission, g/100sq in.
- Red Fuming Nirtric Acid Transmission, g/100sq in.
- Salt Spray Resistance on aluminum, Hours
- Salt Spray Resistance on steel, Hours
- Sulfuric Acid Transmission, g/100sq in.
- Water Transmission, g/100sq in.
- Weather Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|