DuPont Teflon® PTFE Grade 6C Resin for Lubricated Paste Extrusion
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Close Analogs: Data provided by the manufacturer.
Key Words: Polytetrafluoroethylene; DuPont Fluoroproducts
Material Notes: Available in white powder, often called "fine powder," this fluoropolymer resin is capable of being sheared by lubricated paste extrusion (facilitated by a hydrocarbon liquid) into a coherent fibrous matrix with useful structural integrity. Teflon® PTFE fine powders provide a practical method for producing long lengths of product from a resin that cannot be melt extruded. Resin Characteristics: General purpose, medium reduction ratio, excellent color and clarity; accepts filler exceptionally well. Uses: Push/pull cable liner; hose; electrical tape and sleeving; wire and cable coating; unsupported cable; heat-shrinkable tubing. Typical properties for Teflon® PTFE Fine Powder:
| Available Properties |
- Specific Gravity
- Bulk Density
- Water Absorption
- Particle Size
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Coefficient of Friction
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistivity per Square
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Melting Point
- Flammability, UL94
- Oxygen Index
- Drying Temperature
- 20% Hydrochloric Acid Transmission, g/100sq in.
- 50% Sodium Hydroxide Transmission, g/100sq in.
- Acetic Acid Transmission, g/100sq in.
- Acetone Transmission, g/100sq in.
- Acetophenone Transmission, g/100sq in.
- Benzene Transmission, g/100sq in.
- Carbon Tetrachloride Transmission, g/100sq in.
- Chemical/Solvent Resistance
- Detergent Resist. on grit-blasted aluminum, Hours
- Detergent Resistance on aluminum, Hours
- Detergent Resistance on grit-blasted steel, Hours
- Etyl Acetate Transmission, g/100sq in.
- Folding Endurance, # cycles, .18-.20 mm
- Heat of Combustion J/g
- Hexane Transmission, g/100sq in.
- Piperidine Transmission, g/100sq in.
- Red Fuming Nirtric Acid Transmission, g/100sq in.
- Rheometer Pressure, Mpa
- Salt Spray Resistance on aluminum, Hours
- Salt Spray Resistance on steel, Hours
- Sulfuric Acid Transmission, g/100sq in.
- Water Transmission, g/100sq in.
- Weather Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|