DuPont Teflon® PTFE Grade 65 Resin for Lubricated Paste Extrusion
Subcategory: Fluoropolymer; Thermoplastic; PTFE
Close Analogs: Data provided by the manufacturer.
Key Words: Polytetrafluoroethylene; DuPont Fluoroproducts
Material Notes: Available in white powder, often called "fine powder," this fluoropolymer resin is capable of being sheared by lubricated paste extrusion (facilitated by a hydrocarbon liquid) into a coherent fibrous matrix with useful structural integrity. Teflon® PTFE fine powders provide a practical method for producing long lengths of product from a resin that cannot be melt extruded. Resin Characteristics: Low reduction ratio Uses: Thread sealant tape Typical properties for Teflon® PTFE Fine Powder:
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|