DuPont Teflon® PTFE Grade B Filter Fabric Finish

 

Subcategory: Fluoropolymer; Thermoplastic; PTFE

Key Words: Polytetrafluoroethylene; DuPont Fluoroproducts

Material Notes:
Teflon® PTFE B is an aqueous dispersion containing approximately 61%, by total weight, of active ingredients, which include 0.05 to 0.5 mm polytetrafluoroethylene (PTFE) resin particles. It is a milky white liquid with a pH of 8.5.

Compared with other grades of PTFE dispersions, Teflon® PTFE B is a special formulation designed for application to woven glass fabric used to make bags for difficult gaseous filtration or product collection systems. The bags must be self-lubricating and resist clogging for years, while being flexed in high-temperature, corrosive atmospheres.

When properly applied, Teflon® PTFE B improves the flex life, heat and chemical resistance, and antiadhesion behavior of glass fabric, resulting in filter bags with enhanced service life and efficiency.

Applications

Large, high-performance filter bags are made of woven glass fabric treated with Teflon® PTFE B. Principal markets are for pollution control of coal-fired boilers in utility and industrial plants, and for product collection in hostile environments, such as those for producing carbon black.

Available Properties
  • Specific Gravity
  • Solids Content
  • Particle Size
  • pH
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。