DuPont Teflon® PFA Grade 450 HP Extrusion and Molding Resin
Subcategory: Fluoropolymer; Thermoplastic; PFA
Key Words: DuPont Fluoroproducts; DuPont PFA
Material Notes: DuPont™ Teflon® PFA 450 HP fluoropolymer is a special purpose resin available in clear, 2.5-mm (0.1-in.) pellets. This resin is a chemically modified form of Teflon® PFA 350 that combines many of the benefits of the parent resin with several new ones. The additional benefits may include enhanced purity, improved thermal stability while processing and chemical inertness, for example, to ozonated fluids. Similar to Teflon® PFA 350, this resin has a relatively low flow rate, long flex life, and enhanced resistance to enviromental stress cracking compared with most other grades of Teflon® PFA.The enhanced purity of Teflon® PFA 450 HP makes it suitable for applications that require improved color, lower extractable fluorides, and freedom from other foreign materials. This product contains no additives and is designed for hostile chemical environments where purity in the parts-per-billion range is needed. Examples are in semiconductor manufacture, fluid handling systems for industry or life sciences, and instrumentation for precise measurements of fluid systems. Teflon® PFA 450 HP is preferred when extended service is required in hostile environments involving chemical, thermal, and mechanical stress. Table 1 shows the typical property data for Teflon® PFA 450 HP. The improved thermal stability of Teflon® PFA 450 HP results in reduced amounts of bubbles in final parts and decreased corrosion of processing equipment. Teflon® PFA 450 HP combines the processing ease of conventional thermoplastics with properties similar to those of polytetrafluoroethylene. Properly processed products made from neat Teflon® PFA 450 HP resin provide the superior properties typical of fluoropolymer resins: retention of properties after service at 260°C (500°F), useful properties at –196°C (–320°F), and chemical inertness to nearly all industrial chemicals and solvents. Dielectric properties are excellent. Molded products have moderate stiffness and high ultimate elongation. In a flame situation, products of Teflon® PFA 450 HP resist ignition and do not themselves promote flame spread. When ignited by flame from other sources, their contribution of heat is very small and added at a slow rate with very little smoke. Statements, or data, regarding behavior in a flame situation are not intended to reflect hazards presented by this or any other material when under actual fire conditions. Applications Applications for Teflon® PFA 450 HP include tubing; unsupported pipe or pipe linings for production of ultrapure chemicals; semiconductor component handling systems and fluid handling components.
| Available Properties |
- Specific Gravity
- Water Absorption
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Flexural Modulus
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistivity per Square
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Melting Point
- Maximum Service Temperature, Air
- Flammability, UL94
- Oxygen Index
- Drying Temperature
- 20% Hydrochloric Acid Transmission, g/100sq in.
- 50% Sodium Hydroxide Transmission, g/100sq in.
- Acetic Acid Transmission, g/100sq in.
- Acetone Transmission, g/100sq in.
- Acetophenone Transmission, g/100sq in.
- Benzene Transmission, g/100sq in.
- Carbon Tetrachloride Transmission, g/100sq in.
- Chemical/Solvent Resistance
- Etyl Acetate Transmission, g/100sq in.
- Folding Endurance, # cycles, .18-.20 mm
- Heat of Combustion J/g
- Hexane Transmission, g/100sq in.
- Piperidine Transmission, g/100sq in.
- Red Fuming Nirtric Acid Transmission, g/100sq in.
- Salt Spray Resistance on aluminum, Hours
- Sulfuric Acid Transmission, g/100sq in.
- Water Transmission, g/100sq in.
- Weather Resistance
|
|
|
|
| Property Data |
This page displays only the text