DuPont 160 FEP Fluorinated Ethylene Propylene
Subcategory: Fluoropolymer; Thermoplastic; FEP
Close Analogs: Data provided by the manufacturer.
Key Words: DuPont Fluoroproducts; DuPont FEP
Material Notes: DuPont FEP meets the ASTM specification for FEP - Fluorocarbon Molding and Extrusion Materials under ASTM Designation D2116-95a. Has excellent chemical resistance, superior electrical properties, high service temperatures, outstanding low temperature toughness and unique flame resistance. Processed by conventional melt-extrusion and molding techniques. Resin Characteristics: Premium resin with enhanced ESCR. Lowest melt flow rate of 100 series. Uses: Films; chemical linings; large heat-shrinkable tubing for roll covers; high-stress applications
| Available Properties |
- Specific Gravity
- Water Absorption
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Coefficient of Friction
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistivity per Square
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- Melting Point
- Flammability, UL94
- Oxygen Index
- Drying Temperature
- 20% Hydrochloric Acid Transmission, g/100sq in.
- 50% Sodium Hydroxide Transmission, g/100sq in.
- Acetic Acid Transmission, g/100sq in.
- Acetone Transmission, g/100sq in.
- Acetophenone Transmission, g/100sq in.
- Benzene Transmission, g/100sq in.
- Carbon Tetrachloride Transmission, g/100sq in.
- Chemical/Solvent Resistance
- Detergent Resist. on grit-blasted aluminum, Hours
- Detergent Resistance on aluminum, Hours
- Detergent Resistance on grit-blasted steel, Hours
- Etyl Acetate Transmission, g/100sq in.
- Folding Endurance, # cycles, .18-.20 mm
- Heat of Combustion J/g
- Hexane Transmission, g/100sq in.
- Piperidine Transmission, g/100sq in.
- Red Fuming Nirtric Acid Transmission, g/100sq in.
- Salt Spray Resistance on aluminum, Hours
- Sulfuric Acid Transmission, g/100sq in.
- Water Transmission, g/100sq in.
- Weather Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|