DuPont Teflon® FEP CX5010 Fluoropolymer Resin

 

Subcategory: Fluoropolymer; Thermoplastic; FEP

Key Words: DuPont Fluoroproducts; DuPont FEP

Material Notes:
The CX/FR range of Teflon® FEP fluoropolymer resins consists of a Teflon® FEP fluoropolymer with a nucleating system compounded into it. Teflon® FEP CX5010 is Teflon® FEP 100 based while Teflon® FR5020 and FR5030 are Teflon® FEP 5100 based. The nucleating systems are designed to give the foaming characteristics needed for a wide range of primary wire conductor insulation performance.

Supplied as white pellets, these resins are used in conventional foam extrusion processes with the addition of nitrogen gas to produce foamed dielectric insulations. The product range is formulated to allow the cable designer to use them in a wide range of design dimensions and electrical performances. The particles in the nucleating packages compounded into these resins act as initiation sites for foam cells. These foam cells are formed when nitrogen, which is absorbed in the melted resin, expands as pressure is relieved when the melt exits the wirecoating crosshead. Teflon® FEP CX5010, FR5020 and FR5030 are listed in order of ascending nucleating efficiency. Foaming FEP enhances its electronic properties, providing opportunities for miniaturization and weight savings.

Teflon® FEP CX5010 is ideal for producing coaxial cable cores in a broad range of sizes. The core diameters can vary from 0.05 in. (1.27 mm) to 0.50 in. (12.7 mm). Foamed coaxial cables of Teflon® FEP CX5010 are known for high-frequency signal transmission with minimal distortion. A typical coaxial cable core made from Teflon® FEP CX5010 contains up to 60 percent voids. These voids are closedcell in nature and range from 0.001 in. (0.025 mm) to 0.010 in. (0.25 mm) in diameter. Teflon® FEP CX5010 has an MFR range of 6.4 to 7.5.

Teflon® FEP FR5020 is an excellent material for producing the foamed primary dielectric insulation in a cable that possesses an overall shield or shields on each twisted pair in that cable. The primary core diameters can vary from 0.05 in. (1.27 mm) to 0.10 in. (2.54 mm). Foamed insulation primaries of Teflon® FEP FR5020 are known for highfrequency signal transmission with minimal distortion. These foam cores may contain 20 to 40 percent voids. These voids are closed cell in nature and range from 0.0007 in. (0.018 mm) to 0.002 in. (0.05 mm) in diameter. Teflon® FEP FR5020 and FR5030 have an MFR range of 19 to 25.

Teflon® FEP FR5030 is an excellent material for producing the foamed primary dielectric insulation in a cable that possesses unshielded twisted pairs. It is the most efficient nucleated FEP compound in the range. Cable primary core diameters can vary from ,0.035 in. (0.89 mm) to 0.050 in. (1.27 mm). Foamed insulation primaries of Teflon® FEP FR5030 are known for high-frequency signal transmission with minimal distortion. These foam cores may contain 20 to 40 percent voids. These voids are closed cell in nature and range from 0.0007 in. (0.018 mm) to 0.0013 in. (0.033 mm) in diameter.

Available Properties

We're sorry, but our sources do not report
any other information for this material.

  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。