DuPont Tefzel® 2195 Fluoropolymer Resin
Subcategory: Fluoropolymer; Thermoplastic; ETFE/ECTFE
Key Words: Ethylene Tetrafluoroethylene Copolymer; DuPont Fluoroproducts
Material Notes: DuPont™ Tefzel ® 2195 fluoropolymer is a premium-grade resin designed for use in rotational molding. To be effective as a rotational molding resin, Tefzel ® 2195 is a free-flowing powder, with controlled particle size, shape, and size distribution. The properties of Tefzel ® 2195 in molded form are similar to other grades of Tefzel ® fluoropolymer resin. Table 1 shows typical property data for Tefzel ® 2195.Rotational molding is a favored process for making hollow parts (particularly large parts) or for parts with complex geometries. Depending on part design and processing conditions, Tefzel ® 2195 can also be used to rotoline items, whereby the Tefzel® binds to the inner surface of the part to form a lining. Properly processed rotational moldings made from Tefzel ® 2195 provide the superior properties typical of the fluoropolymer resins: retention of properties after service at 150°C (302°F), useful properties at –100°C (–148°F), and chemical inertness to most industrial chemicals and solvents. Molded products have excellent stiffness and high ultimate elongation. Statements, or data, regarding behavior in a flame situation are not intended to reflect hazards presented by this or any other material when under actual fire conditions. Applications Tefzel ® 2195 is ideal for many end products for fluid handling in the chemical processing industries, including pump housings, vessels, columns, elbows, tees, and pipe sections with unusual shapes. In addition, any hollow structure with internal contours that permits uniform coating by powder flow is a candidate for lining, provided it can withstand high temperatures.
| Available Properties |
- Specific Gravity
- Bulk Density
- Water Absorption
- Particle Size
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Coefficient of Friction
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistivity per Square
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Flammability, UL94
- Oxygen Index
- Drying Temperature
- 20% Hydrochloric Acid Transmission, g/100sq in.
- 50% Sodium Hydroxide Transmission, g/100sq in.
- Acetic Acid Transmission, g/100sq in.
- Acetone Transmission, g/100sq in.
- Acetophenone Transmission, g/100sq in.
- Benzene Transmission, g/100sq in.
- Carbon Tetrachloride Transmission, g/100sq in.
- Chemical/Solvent Resistance
- Etyl Acetate Transmission, g/100sq in.
- Folding Endurance, # cycles, .18-.20 mm
- Heat of Combustion J/g
- Hexane Transmission, g/100sq in.
- Piperidine Transmission, g/100sq in.
- Red Fuming Nirtric Acid Transmission, g/100sq in.
- Salt Spray Resistance on aluminum, Hours
- Sulfuric Acid Transmission, g/100sq in.
- Water Transmission, g/100sq in.
- Weather Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|