DuPont Tefzel® HT-2004 25% Glass Reinforced Tefzel®
Subcategory: Fluoropolymer; Thermoplastic; ETFE/ECTFE
Key Words: Ethylene Tetrafluoroethylene Copolymer; DuPont Fluoroproducts
Material Notes: The development of technology by DuPont for reinforcing Tefzel ® ETFE fluoropolymer with glass fibers brings to the plastics industry a new opportunity for design. This product, designated Tefzel ® HT-2004, combines the superior mechanical properties resulting from glass-reinforcement with the impressive thermal, chemical, and electrical properties of Tefzel ®.
| Available Properties |
- Specific Gravity
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Coefficient of Friction
- Izod Impact, Notched
- Dielectric Strength
- CTE, linear 20°C
- Flammability, UL94
- Chemical/Solvent Resistance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|