DuPont Tefzel® HT-2190 Fluoropolymer Resin

 

Subcategory: Fluoropolymer; Thermoplastic; ETFE/ECTFE

Key Words: Ethylene Tetrafluoroethylene Copolymer; DuPont Fluoroproducts

Material Notes:
DuPont™ Tefzel® HT-2190 fluoropolymer resin is a premium grade resin designed for use in rotational mmolding. In order to be effective as a rotational molding resin, HT-2190 is a free-flowing powder, with controlled particle size, shape, and size distribution.

The properties of Tefzel® HT-2190 in molded form are similar to other grades of Tefzel® fluoropolymer resin. Table 1 shows typical property data for Tefzel® HT-2190.

Rotational molding is a favored process for making hollow parts (particularly large parts) or for parts with complex geometries. Depending on part design and processing conditions, Tefzel® HT-2190 can also be used to rotoline items, in which process the Tefzel® is bound to the inner surface of the part, thus forming a lining.

Properly processed rotational moldings made from Tefzel® HT-2190 provide the superior properties typical of the fluoropolymer resins: retention of properties after service at 150°C (302°F), useful properties at –100°C (–148°F), and chemical inertness to most industrial chemicals and solvents. Dielectric properties are excellent. Molded products have excellent stiffness and high ultimate elongation. Statements, or data, regarding behavior in a flame situation are not intended to reflect hazards presented by this or any other material when under actual fire conditions.

Applications

Tefzel® HT-2190 is ideal for many end products for fluid handling in the chemical processing industries, including pump housings, vessels, columns, elbows, tees, and pipe sections with unusual shapes. In addition, any hollow structure with internal contours that permit uniform coating by powder flow is a candidate for lining, provided it can withstand high temperatures.

Available Properties
  • Specific Gravity
  • Bulk Density
  • Water Absorption
  • Melt Flow
  • Dielectric Strength
  • CTE, linear 20°C
  • Melting Point
  • Maximum Service Temperature, Air
  • Oxygen Index
  • Chemical/Solvent Resistance
  • Weather Resistance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。