DuPont Kapton® 100A Polyimide Film, 25 Micron Thickness
Subcategory: Polyimide, TS; Thermoset; Polymer
Material Notes: Film thickness 25 micron (1.0 mil) Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications. General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dianhydride with an aromatic diamine. It has excellent chemical resistance; there are no known organic solvents for the film. It does not melt. It can be used at both high and low temperature extremes. Kapton® polyimide films can be used in a variety of electrical and electronic uses: wire and cable tapes, formed coil insulation, substrates for printed circuit boards, motor slot liners, magnet wire insulation, transformer and capacitor insulation, magnetic and pressure-sensitive tapes, and tubing. Data provided by DuPont High Performance Films.
| Available Properties |
- Density
- Water Absorption
- Film Tensile Strength at Break, MD
- Film Elongation at Break, MD
- Poissons Ratio
- Secant Modulus
- Coefficient of Friction
- Coefficient of Friction, Static
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Glass Temperature
- Flammability, UL94
- Refractive Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|