DuPont Kapton® 250FN029 Polyimide/FEP Composite Film
Subcategory: Polyimide, TS; Thermoset; Polymer
Material Notes: 250 Gauge film structure consisting of a 50 µm (2 mil) base polyimide film with a 13 µm (0.5 mil) coating of Teflon® FEP on one side. Kapton® Type HN film coated with Teflon® FEP fluoropolymer resin, imparts heat sealability, provides a moisture barrier, and enhances chemical resistance. General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dianhydride with an aromatic diamine. It has excellent chemical resistance; there are no known organic solvents for the film. It does not melt. It can be used at both high and low temperature extremes. Kapton® polyimide films can be used in a variety of electrical and electronic uses: wire and cable tapes, formed coil insulation, substrates for printed circuit boards, motor slot liners, magnet wire insulation, transformer and capacitor insulation, magnetic and pressure-sensitive tapes, and tubing. Data provided by DuPont High Performance Films.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Moisture Vapor Transmission
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Break, MD
- Film Elongation at Break, MD
- Secant Modulus
- Impact Test
- Tear Strength Test
- Elmendorf Tear Strength MD
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Specific Heat Capacity
- Thermal Conductivity
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|