DuPont Kevlar® 29 Aramid Fiber
Subcategory: Aramid; Thermoset; Composite Fibers
Material Notes: 1500 Denier; 1000 Filaments. General KEVLAR Information: DuPont Kevlar® poly-para-phenylene terephthalamide (aramid) has a unique combination of high strength, high modulus, toughness, and thermal stability. It was developed for demanding industrial and advanced-technology applications. It is chemically stable under a wide variety of exposure conditions; however, certain strong aqueous acids, bases, and sodium hypochlorite can cause degradation, particularly over long periods of time and at elevated temperatures. Information provided by DuPont.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Tensile Strength, Ultimate
- Tenacity
- Elongation at Break
- Tensile Modulus
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|